We present, to the best of our knowledge, the first intracavity pumped Yb:YAG thin-disk laser. It operates at 1050.7 nm with a quantum defect of just 1.74% due to pumping at 1032.4 nm. Low absorption of the pump light at the pump wavelength of 1032.4 nm is compensated for by placing the disk inside the resonator of another Yb:YAG thin-disk laser which is diode-pumped at 940 nm. The intra-cavity pumped laser has an output power of 10.3 W and a slope efficiency of 8.3%
We report interferometric measurements of the temperature coefficient of the refractive index (dn=dT) and the coefficient of thermal expansion (a) of a praseodymium-doped yttrium lithium fluoride (Pr:YLF) crystal and of a fused silica reference sample. Our phase-resolved interferometric method yields a large number of data points and thus allows a precise measurement and a good error estimation. Furthermore, both dn=dT and a are obtained simultaneously from a single measurement which reduces errors that can occur in separate measurements. Over the temperature range from 20 °C to 80 °C, the value of dn=dT of Pr:YLF decreases from -5.2 x 10-6 /K to -6.2 x 10-6 /K for the ordinary refractive index and from -7.6 x 10-6 /K to -8.6 x 10-6 /K for the extraordinary refractive index. The coefficient of thermal expansion for the a-axis of Pr:YLF increases from 16.4 x 10-6 /K to 17.8 x 10-6 /K over the same temperature range.